Grade | Thickness | C max | Mn | P max | S max | Si | Cu max | Ni max | Cr max | Mo max |
A537 Class 1 | t≤40 | 0.24 | 0.70-1.35 | 0.025 | 0.025 | 0.15-0.50 | 0.35 | 0.25 | 0.25 | 0.08 |
40﹤t | 1.00-1.60 |
Class | Thickness | Heat treatment | Tensile strength Rm MPa | Yield strength ReH MPa min | Elongation A% min |
A537 Class 1 | t≤65 | Normalized | 480-620 | 345 | 22 |
65﹤t≤100 | 450-585 | 310 | |||
100﹤t≤150 | - | - | 18 |
Other grades of steel plates for pressure vessel and boiler equipment in standard ASTM A537/A537M and ASME SA537/SA537M:
A537 Class 2 pressure vessel steel plates,
A537 Class 3 pressure vessel steel plates,
SA537 Class 1 pressure vessel steel plates,
SA537 Class 2 pressure vessel steel plates,
SA537 Class 3 pressure vessel steel plates