W.Nr.2.4669 alloy steel

Share:

W.Nr.2.4669 Alloy steel is mainly by γ [Ni3 (Al, Ti, Nb)] phase of nickel base superalloy aging strengthening, has good corrosion resistance and oxidation resistance at 980 degree, 800 degree with higher intensity, 540 degree with relaxation has good performance, but also has the forming and welding performance good. This alloy is mainly used in the manufacture of aero engine under 800 degree and requirements and high strength corrosion resistant ring parts, structural parts and bolts and other components, in 540 degree work with medium or low stress and resistance to planar spring relaxation and spiral spring. Also can be used in the manufacture of gas turbine blades. Can supply a variety of sheet, strip, bars, forgings, ring, wires and tubes.

W.Nr.2.4669 Wrounght nickel-base superalloy equal material :W.Nr.2.4669,NiCr15Fe7TiAl NCF750,UNS N07750

W.Nr.2.4669 Alloy steel Chemical composition


C

Cr

Ni+Co

Al

Ti

Fe

Nb+Ta

Co

Mn

Si

S

Cu

P

≤0.08

14.0-17.0

≥70.0

0.40-1.00

2.25-2.75

5.00-9.00

0.70-1.20

1.00

1.00

0.50

0.010

0.50

0.015

W.Nr.2.4669 Alloy steel physical properties
W.Nr.2.4669 Alloy steel The melting temperature range 1395-1425 degree.
W.Nr.2.4669 Alloy steel Density : 8.25g/cm3

InconelX-750 alloy steel Mechanical properties

Product

Tensile strength /MPa

Yield strength MPa

Elongation /%

HRC

W.Nr.2.4669 Alloy steel Strip

≤930

-

≥18

-

≥1105

-

≥12

≥30

W.Nr.2.4669 Alloy cold rolled steel sheet

≤930

≤515

≥30

-

≤930

≤515

≥35

-

W.Nr.2.4669 Alloy hot rooled steel plate

≥1170

≥795

≥18

≥32

W.Nr.2.4669 Alloy steel tube

≤965

≤550

≥35

-

≥1170

≥790

≥15

-